Call Us
Customer Support & Sales
+919996186555
Creep Testing Unit

Creep Testing Unit

Product Details:

X

Product Description

Creep Testing Unit

Specification

[1] Table unit for the investigation of the creep behaviour of different materials

[2] Flat specimens made of lead and PE

[3] Specimen cross-section 2x5mm, measured length 25mm

[4] Tensile stress range 5...25N/mm²

[5] Position measurement gauge 0...10mm, resolution 0.01mm

[6] Experiments above or below room temperature possible with conditioning box

Technical Data

Specimen

material: lead, PE

cross-section: 2x5mm

measured length: 25mm

Tensile stress range: 5...25N/mm²

Position measurement

range: 0...10mm

resolution 0.01mm